MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese VECTRAN™ V200P Co-Extrudable Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Description: PRELIMINARY DATA SHEET: Co-extrudable LCP for Barrier Applications. Vectran V200P is not suitable for medical or dental implants.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Moisture Absorption at Equilibrium 0.020 %at 50% RH; ISO 62
Moisture Vapor Transmission 0.0154 cc-mil/100 in²-24hr-atmat 38°C; DIN 53122-2
Oxygen Transmission 0.0390 cc-mil/100 in²-24hr-atm73°F, 100%RH; DIN 53380 part 3
 0.0420 cc-mil/100 in²-24hr-atm73°F, 0% RH; DIN 53380 part 3
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 182 MPa5 mm/min; ISO 527-2/1A
Elongation at Break 3.4 %5 mm/min; ISO 527-2/1A
Tensile Modulus 10.6 GPa1 mm/min; ISO 527-2/1A
Flexural Strength 158 MPaISO 178
Flexural Modulus 9.10 GPaISO 178
Izod Impact, Notched (ISO) 95.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) 252 kJ/m²ISO 180/1U
Charpy Impact Unnotched 26.7 J/cm²ISO 179/1eU
Charpy Impact, Notched 9.50 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 187 °CISO 75-1, -2
Deflection Temperature at 8.0 MPa 94.0 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 245 - 255 °C
Middle Barrel Temperature 265 - 275 °C
Front Barrel Temperature 285 - 295 °C
Die Temperature 545 - 563 °F
Melt Temperature 285 - 295 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese VECTRAN™ V100P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese VECTRAN™ V400P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese VECTRAN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese VECTRA® 1300MT Medical Grade Liquid Crystal Polymer (LCP)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

PHCV57 / 45898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.