MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Synprene™ RT-5190 RoHS Black Styrene Butadiene Block Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastomers. These materials are ideal for applications requiring flexibility over a wide temperature range, excellent colorability, broad processing capability and durability.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 9010 sec; ASTM D2240
Tensile Strength at Break 13.8 MPa510 mm/min; ASTM D412A
Tensile Stress at Strain 7.93 MPa
@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break >= 500 %510 mm/min; ASTM D412A
Resilience 37Bayshore Resilience, %; ASTM D2632
Tear Strength 58.7 kN/mDie C, 510 mm/min; ASTM D624
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -50.0 °CASTM D746
Flammability, UL94 V-0
@Thickness 1.59 mm
NC; UL 94
Oxygen Index 27 %
@Thickness 1.57 mm
ASTM D2863
 
Descriptive Properties
AppearanceNatural Color
FeaturesFlame Retardant
 General Purpose
FormsPellets
Generic MaterialSBC
Generic NameStyrene Butadiene Block Copolymer (SBC)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 Consumer Applications
 Industrial Applications
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Synprene™ RT-5155 RoHS Natural Styrene Butadiene Block Copolymer (SBC)
Avient Elastamax™ XL 0131-59 Styrene Butadiene Block Copolymer (SBC)
Avient Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC)
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded

PH0POL0099 / 144668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.