Product Description: Bicor ARW is a two-side acrylic-coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher COF is intended to be against the paper to ensure a tight wrap, whereas the side with the lower COF is intended as the outside surface. This film has broad seal range suitable for ream overwrap applications. Availability: Latin America, North America and South America Key Features: - Consistent COF
- Robust machinability
- Excellent optical properties
- Good hot slip
- Excellent stiffness
- Excellent hot melt adhesion
- Excellent hot tack and seal strength
- Excellent flavor and aroma barrier
Features:- Acrylic Coated
- Broad seal Range
- In Lamination Lap Sealable
Applications:Uses:- Box Overwrap Flexible Packaging
- HFFS Flexible Packaging
- Pre-made Bags – Flexible Packaging
- Tobacco Overwrap Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination and Surface Print UnsupportedInformation provided by ExxonMobil |