MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ExxonMobil Metallyte™ 28UBW-ES OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A multi-layer, cavitaed, white OPP film with an enhanced sealant to allow sealing through contamination. This film has an exceptional barrier to gases, flavors, and moisture. It is metalized on one side with a proprietary sealant layer on the other. 28UBW-ES is lap sealable to other coextruded OPP films.

Availability: Latin America, North America and South America

Key Features:

  • Very low MST, broad seal range
  • Outstanding opacity
  • Outstanding moisture and oxygen barrier
  • Outstanding aroma and flavor barrier
  • Excellent flex-Crack resistance
  • Excellent hot tack
Features:
    Flavor & Aroma Barrier
  • Gas Barrier
  • In Lamination Lap Sealable
  • Light Barrier
  • Moisture Barrier
  • Oxygen Barrier
Applications:
  • Dry Foods and Beverage Powders
Uses:
  • HFFS Flexible Packaging
  • Pouches – Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Priming, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 0.101 g/m²/day
@Temperature 38.0 °C
0.00650 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate 0.0931 cc/m²/day0.00600 cc/100 in²/dayExxonMobil Method
Thickness 27.9 microns1.10 milExxonMobil Method
Coating Weight 20.3 g/m²12.7 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Break, MD 82.7 MPa12000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 172 MPa25000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
5.0 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C
3.0 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Optical Density 3.03.0ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST175°FUntreated
Crimp Seal Strength1500 g/inUntreated, 260°F, 20 psi, 0.8 sec
 700 g/inUntreated, 210°F, 20 psi, 0.8 sec
Yield34000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Bicor™ 18MB090 OPP Film
ExxonMobil Bicor™ 30MBR666 OPP Film
ExxonMobil Bicor™ 21MB621 OPP Film
ExxonMobil Bicor™ 25 ARW OPP Film
ExxonMobil Bicor™ 15MB440 OPP Film

PEX99528 / 175764

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.