MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

X12CrNi177 Austenitic Stainless Steel for medical instruments
Categories: Metal; Ferrous Metal; Austenitic; Special-Purpose Steel; Stainless Steel

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 515 MPa74700 psiAnnealed
 1280 MPa186000 psiFull hard
Tensile Strength, Yield 205 MPa29700 psiAnnealed
 965 MPa140000 psiFull hard
Elongation at Break 9.0 %9.0 %Full hard
 40 %40 %Annealed
Modulus of Elasticity 193 GPa28000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 70.0 - 300 °C
9.44 µin/in-°F
@Temperature 158 - 572 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 16.2 W/m-K112 BTU-in/hr-ft²-°F
 
Descriptive Properties
Magnetic PropertiesParamagnetic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for T 600 Series Stainless Steel
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel, condition H1025
BASF Ultramid® A3EG7 BK00564 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3K BK00464 PA66 (Dry)
BASF Ultramid® A3X2G5 BK23187 25% Glass Filled PA66 (Dry)

MMEDIC05 / 12381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.