MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3X2G5 BK23187 25% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Ultramid A3X2G5 BK23187 is a 25% glass fiber reinforced, pigmented black injection molding PA66 grade with improved flame retardance and enhanced long-term performance. Flame retardant based on red phosphorus; outstanding mechanical and electrical properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Water Absorption 6.0 %6.0 %ISO 62
Moisture Absorption at Equilibrium 1.4 %1.4 %23°C/50% R.H.; ISO 62
Melt Flow 40 g/10 min
@Load 5.00 kg,
Temperature 275 °C
40 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 115 MPa16700 psi5mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527
Flexural Modulus 6.90 GPa1000 ksiISO Data
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO Test
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Strength 33.0 kV/mm838 kV/inIEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10 K/min
 260 °C500 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Descriptive Properties
ColorBK23187
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry)
X12CrNi177 Austenitic Stainless Steel for medical instruments
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel, condition H1025
BASF Ultramid® A3K BK00464 PA66 (Dry)
BASF Ultramid® A3EG7 BK00564 35% Glass Filled PA66 (Dry)

PBASF9271 / 85035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.