MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical LUTENE LB5000 LDPE Extrusion Coating
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Description: LUTENE LB5000 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB5000 is also noted for the excellent adhesion to porous and non porous substrates such as paper, nylon, OPP, PET and aluminum and has good heat seal strength and hot-tack strength. LUTENE LB5000 contains on additives.

Main Application: Flexible package( tie layer or sealant layer of laminating film), paper and paper board coating (release paper, paper cup, kraft paper)

CAS No. 9002-88-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.918 g/cc0.918 g/ccASTM D1505
Water Vapor Transmission 20.0 g/m²/day
@Pressure 0.101 MPa
1.29 g/100 in²/day
@Pressure 14.7 psi
ASTM D393
Melt Flow 5.0 g/10 min
@Load 2.61 kg,
Temperature 190 °C
5.0 g/10 min
@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4343ASTM D2240
Tensile Strength at Break 12.0 MPa1740 psi200mm/min; ASTM D638
Tensile Strength, Yield 8.83 MPa1280 psi200 mm/min; ASTM D638
Elongation at Break 550 %550 %200 mm/min; ASTM D638
Flexural Modulus 0.196 GPa28.4 ksi200mm/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 107 °C225 °F10°C/min; DSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin
Braskem BC818 Extrusion Coating Low Density Polyethylene
Carmel Olefins Ipethene® 111 Low Density Polyethylene

PLAY217 / 148227

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.