MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Omnia Plastica Rilsan® PA6 GF - Akulon GF - at 50% RH
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitable for gears and mechanical parts where excellent wear resistance is required.

Features:

  • Very high wear resistance: this inherent polyamide feature is further increased by the addition of glass. Akulon GF is one of the best wear resistant plastic materials available.
  • High compression strength and tensile stress: the fatigue resistance is excellent as are the general mechanical properties.
  • Ageing resistance: weatherproof and good resistance at low temperature
  • Black colour.

Weak Point:

If used in combination with moving parts, the glass filler causes abrasion of the steel parts in contact with the plastic.

Application:

  • Mechanical: very high compressive strength and wear resistance, in fact one the best of all the engineering plastics. This material is particularly suitable for gears and high performance mechanical components which need to operate in demanding environments, such as on construction equipment or earthmovers, without suffering from excessive wear.
  • Food contact: it cannot be used in contact with food.
  • Electrical: even though the electrical properties change with the moisture content, this nylon is still used where good mechanical features as well as weatherproof performance are required.
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 2.0 %2.0 %50% relative humidity (beginning dry)
Water Absorption at Saturation 5.2 %5.2 %23°C (beginning dry)
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 170 MPa24700 psiISO2039.1 DIN.53456
Tensile Strength at Break 100 MPa14500 psiISO.527 DIN.53455
Elongation at Break 20 %20 %ISO.527 DIN.53455
Tensile Modulus 4.00 GPa580 ksiISO.527 DIN.53455
Compressive Strength 15.0 MPa2180 psi1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NBNB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.500.50on dry ground steel; load =0.05MPa; speed =0.6 m/s (dry sample)
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 7.0
@Frequency 1e+6 Hz
7.0
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 140 °F
dry sample
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FDIN.52612 (dry sample)
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 105 °C221 °FContinuous; 5000 hours based on a tensile stress of 50% at 23° C. (dry sample)
 170 °C338 °Fshort period, no load (dry sample)
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FISO.75 DIN.53461 (dry sample)
Minimum Service Temperature, Air -30.0 °C-22.0 °Fimpact conditions and heavy loads not considered (dry sample)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450GL30 30% Glass Fiber Reinforced
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
Fibre Glast 77 Wax-Free General Purpose Polyester Molding Resin
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)

POMNIA23 / 55616

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.