MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee WC20 Cerium Oxide-doped Tungsten
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Non-radioactive material for welding electrodes

Characteristics (compared to pure tungsten):

  • Lower electron work function
  • Improved ignition characteristics
  • Longer service life

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 19.0 g/cc19.0 g/ccCalculated
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 164 W/m-K1140 BTU-in/hr-ft²-°Fcomparable to pure W
 
Processing PropertiesMetricEnglishComments
Recrystallization Temperature 1560 °C2840 °FDeformation level - 90%
 2600 °C4710 °FDeformation level - 99.99%
 
Component Elements PropertiesMetricEnglishComments
Other, each 2.0 %2.0 %Cerium Oxide
 
Descriptive Properties
Creep Resistancegreater than pure W
Ductilitygreater than pure W
Fineness of Graingreater than pure W
Machinability/Workabilitymuch greater than pure W
Stability at High Temperaturegreater than pure W

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plansee W-20Cu Tungsten-Copper Composite
Plansee WCu22 WCu (80:20)
Plansee W-15Cu Tungsten-Copper Composite
Plansee W-10Cu Tungsten-Copper Composite
NAECO® ELKON® R32 Tungsten Copper material ASTM B702

NPLAM924 / 135480

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.