MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beryllium-Copper Casting Alloy 245C, UNS C82600, Cast and Aged
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Investment, Permanent Mold, Plaster, and Sand.

Applications: Bearings and molds for plastic parts.

Test specimen: cast and aged 3 hours at 345°C.

Key Words: BeCu; beryllium copper 245C, FED QQ-C-390
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.16 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 31
Tensile Strength, Ultimate 825 MPa
Tensile Strength, Yield 725 MPa
@Strain 0.2 %
Elongation at Break 2.0 %In 50 mm
Modulus of Elasticity 130 GPa
Poissons Ratio 0.30
Shear Modulus 50.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000907 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 100 W/m-K
@Temperature 20.0 °C
Melting Point 835 °CIncipient
 855 - 955 °C
Solidus 855 °C
Liquidus 955 °C
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Solution Temperature 790 - 800 °C
Aging Temperature 345 °C
Casting Temperature 980 - 1040 °CHeavy castings
 1040 - 1150 °CLight castings
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.15 %
Beryllium, Be 2.25 - 2.45 %
Chromium, Cr <= 0.10 %
Cobalt, Co 0.35 - 0.70 %
Copper, Cu >= 95.2 %
Iron, Fe <= 0.25 %
Lead, Pb <= 0.020 %
Nickel, Ni <= 0.20 %
Silicon, Si 0.20 - 0.35 %
Tin, Sn <= 0.10 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Copper 21C UNS C82510 Casting Alloy Cast and Aged
Beryllium Copper Alloy 10C, UNS C82000 Cast and Aged
Beryllium-Copper Alloy 20C, UNS C82500, Cast and Aged
Beryllium-Copper Alloy 30C, UNS C82200, Cast and Aged
Beryllium-Copper Casting Alloy 245C, UNS C82600, As-Cast

MC82600b3 / 11890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.