MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beryllium-Copper Casting Alloy 245C, UNS C82600, As-Cast
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Investment, Permanent Mold, Plaster, and Sand.

Applications: Bearings and molds for plastic parts.

Test specimen: as cast.

Key Words: BeCu; beryllium copper 245C, FED QQ-C-390
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.16 g/cc0.295 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8686
Tensile Strength, Ultimate 550 MPa79800 psi
Tensile Strength, Yield 345 MPa
@Strain 0.2 %
50000 psi
@Strain 0.2 %
Elongation at Break 10 %10 %In 50 mm
Modulus of Elasticity 130 GPa18900 ksi
Poissons Ratio 0.300.30
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 50.0 GPa7250 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000907 ohm-cm
@Temperature 20.0 °C
0.0000907 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 100 W/m-K
@Temperature 20.0 °C
694 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 835 °C1540 °FIncipient
 855 - 955 °C1570 - 1750 °F
Solidus 855 °C1570 °F
Liquidus 955 °C1750 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Solution Temperature 790 - 800 °C1450 - 1470 °F
Aging Temperature 345 °C653 °F
Casting Temperature 980 - 1040 °C1800 - 1900 °FHeavy castings
 1040 - 1150 °C1900 - 2100 °FLight castings
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.15 %<= 0.15 %
Beryllium, Be 2.25 - 2.45 %2.25 - 2.45 %
Chromium, Cr <= 0.10 %<= 0.10 %
Cobalt, Co 0.35 - 0.70 %0.35 - 0.70 %
Copper, Cu >= 95.2 %>= 95.2 %
Iron, Fe <= 0.25 %<= 0.25 %
Lead, Pb <= 0.020 %<= 0.020 %
Nickel, Ni <= 0.20 %<= 0.20 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Tin, Sn <= 0.10 %<= 0.10 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Beryllium-Copper Alloy 20C, UNS C82500, As Cast
Beryllium-Copper Alloy 30C, UNS C82200, As-Cast
Beryllium-Copper Alloy 165C, UNS C82400, TB00 Temper
Beryllium-Copper Alloy 50C, UNS C81800, As-cast
Beryllium-Copper Casting Alloy 245C, UNS C82600, Cast and Aged

MC82600b2 / 11889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.