MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aptek DI-STRATE 1500-1 Microwave/RF Foam Substrate
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset

Material Notes: DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.

Uses: Iridium Satellite Antennas

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.270 g/ccFoam
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
Compressive Yield Strength 850 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.97
@Frequency 2.00e+9 Hz
Dissipation Factor 0.0050
@Frequency 2.00e+9 Hz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
Evonik SOLIMIDE® AC-550 Polyimide Foam
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Touchstone CFOAM® 30 Structural Carbon Foam
Aptek DI-STRATE 1503 Microwave/RF Foam Substrate

PAPTEK43 / 24205

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.