MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik SOLIMIDE® AC-550 Polyimide Foam
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: SOLIMIDE AC-550 foam is utilized in aircraft and aerospace markets as a lightweight, non-wicking, fire resistant, thermal and acoustic insulation material. Fuselage, air conditioning duct, and equipment insulation are a few of the applications for SOLIMIDE AC-550 foam. If needed to meet end user requirements, SOLIMIDE AC-550 foam can be faced or coated and cut into a variety of shapes or sizes.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00710 g/cc0.000257 lb/in³ASTM D3574
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.00480 MPa0.696 psi25% Compression; ASTM D3574
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0430 W/m-K0.298 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 200 °C392 °F
 
Descriptive Properties
Content<1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay AVIMID® R Polyimide Composite
Evonik SOLIMIDE® Densified HT Foam
Evonik SOLIMIDE® HT 340 Polyamide Foam
Evonik SOLIMIDE® AC-530 Polyimide Foam
Solvay AVIMID® N Polyimide Composite

PEVONIL661 / 196865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.