Cossa Polimeri ESTACARB 1560 V0 HF Flame Retardant Polycarbonate
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Unreinforced, Flame Retardant
Material Notes:
Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistance
Information provided by Cossa Polimeri S.r.l.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.20
g/cc
0.0434
lb/in³
ASTM D 792
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ASTM D 955
Melt Flow
15
g/10 min
@Load 1.20 kg,
Temperature 300 °C
15
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
60.0
MPa
8700
psi
ASTM D 638
Tensile Strength, Yield
65.0
MPa
9430
psi
ASTM D 638
Elongation at Break
>= 50 %
>= 50 %
ASTM D 638
Flexural Modulus
2.50
GPa
363
ksi
ASTM D 790
Izod Impact, Notched
5.50
J/cm
@Temperature 0.000 °C
10.3
ft-lb/in
@Temperature 32.0 °F
ASTM D 638
6.00
J/cm
@Temperature 23.0 °C
11.2
ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Thermal Properties
Metric
English
Comments
Hot Ball Pressure Test
135
°C
275
°F
I.E.C. 335-1
Vicat Softening Point
146
°C
@Load 5.00 kg
295
°F
@Load 11.0 lb
50°C/hr; ASTM D 1525
148
°C
@Load 0.999 kg
298
°F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94
V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Glow Wire Test
960
°C
1760
°F
I.E.C. 695-2-1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
E-Polymers TEKAMID® H24M10 MF 10% Heat resistance Dimensional stability PA/ABS Alloy
Overview of materials for Polycarbonate, Molded
LNP Thermocomp® RC-1008 Polyamide 66, Carbon Fiber Reinforcement
Kingfa MAC-451PG Electroplating PC/ABS Alloy
Daicel CEVIAN® A2606 30% GF PA/ABS Alloy, DAM
PCOSSA903 / 156493
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.