MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Elastocon® 2850PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2850PE is FDA compliant and well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 2850PE can be overmolded and coextruded with polyethylene.

Information provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm0.015 - 0.025 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5252ASTM D2240
Tensile Strength 6.41 MPa930 psiASTM D412
Elongation at Break 626 %626 %ASTM D412
100% Modulus 1.73 MPa
@Strain 100 %
251 psi
@Strain 100 %
ASTM D412
Compression Set 16 %
@Temperature 20.0 °C,
Time 79200 sec
16 %
@Temperature 68.0 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Feed Temperature <= 79.4 °C<= 175 °F
Rear Barrel Temperature 166 - 177 °C330 - 350 °F
Front Barrel Temperature 182 - 188 °C360 - 370 °F
Nozzle Temperature 193 - 204 °C380 - 400 °F
Mold Temperature 21.1 - 37.8 °C70.0 - 100 °F
Back Pressure 0.689 - 1.38 MPa100 - 200 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black
Avient Elastamax™ XL 0190-24 SEBS-Based Thermoplastic Elastomer
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer
Polykemi AB POLYelast TPE Z506 Thermoplastic Elastomer, SEBS-based
Elastocon TPE Technologies Elastocon® 8088N Thermoplastic Elastomer

PELASC301 / 142477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.