MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYelast TPE Z506 Thermoplastic Elastomer, SEBS-based
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Polykemi AB

Key Words: Thermoplastic Elastomer, SEBS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.020 cm/cm0.014 - 0.020 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.014 - 0.020 cm/cm0.014 - 0.020 in/inISO 2577
Melt Index of Compound 7.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50
@Time 15.0 sec
50
@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 6.00 MPa<= 870 psiISO/R527
Elongation at Break 725 %725 %ISO/R527
100% Modulus 1.40 MPa
@Strain 100 %
203 psi
@Strain 100 %
ISO/R527
300% Modulus 2.50 MPa
@Strain 300 %
363 psi
@Strain 300 %
ISO/R527
Tear Strength 25.0 kN/m143 pliD624
Compression Set  18 %
@Temperature 23.0 °C,
Time 259000 sec
18 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN 53517
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
DIN 53517
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa72.5 - 218 psi
 
Descriptive Properties
Holding PressureLow
Injection PressureLow
Injection SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black
Avient OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE)
Avient Elastamax™ XL 0190-24 SEBS-Based Thermoplastic Elastomer
Elastocon TPE Technologies Elastocon® 2850PE Thermoplastic Elastomer
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural

PPOLYK478 / 123203

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.