MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CHT Group QSil 213 Transparent, Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product Description: QSil 213 is a two-component, clear liquid silicone, which will cure at room temperature or at elevated temperatures. The chemical composition provides hydrolytic stability and reversion resistance. This product is ideal for potting complex parts because it provides electrical insulation and shock resistance.

Key Features:

  • Suitable for automatic dispensing or hand mixing
  • Low viscosity
  • Contains no solvents
  • Non-yellowing catalyst system
  • Designed for superior adhesion with use of primer

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncatalyzed, QSil 213B
 1.02 g/cc1.02 g/ccUncatalyzed, QSil 213A
Viscosity 700 cP700 cPUncatalyzed, QSil 213B
 4000 cP4000 cPUncatalyzed, QSil 213A
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inCured 60 minutes @ 100°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040Cured 60 minutes @ 100°C
Tensile Strength 5.17 MPa750 psiCured 60 minutes @ 100°C
Elongation at Break 100 %100 %Cured 60 minutes @ 100°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cm
Dielectric Constant 2.69
@Frequency 1000 Hz
2.69
@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.0060
@Frequency 1000 Hz
0.0060
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 275 µm/m-°C153 µin/in-°F
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4061.406Cured 60 minutes @ 100°C
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 100 °C
1.00 hour
@Temperature 212 °F
Gel Time 240 min240 minCatalyzed
 
Descriptive Properties
ColorClearUncatalyzed, QSil 213A
 ClearUncatalyzed, QSil 213B
 Clear, colorlessCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Liquid Silicone Rubber
CHT Group QSil 218 Transparent, Liquid Silicone Rubber
BIW Liquid Silicone Rubber, Standard Grades
CHT Group QSil 217 Transparent, Liquid Silicone Rubber

PACC2079 / 199467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.