MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QSil 213 Transparent, Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Product Description: QSil 213 is a two-component, clear liquid silicone, which will cure at room temperature or at elevated temperatures. The chemical composition provides hydrolytic stability and reversion resistance. This product is ideal for potting complex parts because it provides electrical insulation and shock resistance.

Key Features:

  • Suitable for automatic dispensing or hand mixing
  • Low viscosity
  • Contains no solvents
  • Non-yellowing catalyst system
  • Designed for superior adhesion with use of primer

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccUncatalyzed, QSil 213B
 1.02 g/ccUncatalyzed, QSil 213A
Viscosity 700 cPUncatalyzed, QSil 213B
 4000 cPUncatalyzed, QSil 213A
Linear Mold Shrinkage <= 0.0010 cm/cmCured 60 minutes @ 100°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40Cured 60 minutes @ 100°C
Tensile Strength 750 psiCured 60 minutes @ 100°C
Elongation at Break 100 %Cured 60 minutes @ 100°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.70e+15 ohm-cm
Dielectric Constant 2.69
@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm
Dissipation Factor 0.0060
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 275 µm/m-°C
Specific Heat Capacity 0.700 J/g-°C
Thermal Conductivity 0.180 W/m-K
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.406Cured 60 minutes @ 100°C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 100 °C
Gel Time 240 minCatalyzed
 
Descriptive Properties
ColorClearUncatalyzed, QSil 213A
 ClearUncatalyzed, QSil 213B
 Clear, colorlessCatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Liquid Silicone Rubber
CHT Group QSil 218 Transparent, Liquid Silicone Rubber
BIW Liquid Silicone Rubber, Standard Grades
CHT Group QSil 217 Transparent, Liquid Silicone Rubber

PACC2079 / 199467

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.