MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Park Aerospace Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good moisture resistance, as well as excellent tack and drape. Formulated for both oven and autoclave cure, E-752 provides for easy processing with oven cure, without sacrificing mechanical properties.

Key Features and Benefits:

  • Specifically designed to allow both oven cure and autoclave cure
    • Allows oven curing without sacrificing mechanical properties
  • Service temperatures up to 130°C
  • Controlled flow for ease of processing
  • Flexible cure temperature 132°C to 185°C
    • Good mechanical properties can be achieved through oven curing at 132°C, followed by post-cure at 185°C
  • Self-adhesive grade for sandwich panel applications

Applications/Qualifications:

  • Primary and Secondary Aircraft Structures
  • Ducting
  • Fairings
  • Nacelles

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  820 MPa
@Temperature 23.9 °C
119000 psi
@Temperature 75.0 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
 820 MPa
@Temperature 121 °C
119000 psi
@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
 827 MPa
@Temperature 121 °C
120000 psi
@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
Tensile Modulus  65.5 GPa
@Temperature 121 °C
9500 ksi
@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
 65.5 GPa
@Temperature 121 °C
9500 ksi
@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
 66.2 GPa
@Temperature 23.9 °C
9600 ksi
@Temperature 75.0 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
Compressive Strength  319 MPa
@Temperature 23.9 °C
46300 psi
@Temperature 75.0 °F
Open-Hole, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D6484
 607 MPa
@Temperature 121 °C
88000 psi
@Temperature 250 °F
Wet; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
 717 MPa
@Temperature 121 °C
104000 psi
@Temperature 250 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
 827 MPa
@Temperature 23.9 °C
120000 psi
@Temperature 75.0 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
Compressive Modulus  44.8 GPa
@Temperature 23.9 °C
6500 ksi
@Temperature 75.0 °F
Open-Hole, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D6484
 60.0 GPa
@Temperature 121 °C
8700 ksi
@Temperature 250 °F
Wet; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
 61.4 GPa
@Temperature 23.9 °C
8900 ksi
@Temperature 75.0 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
 61.4 GPa
@Temperature 121 °C
8900 ksi
@Temperature 250 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
Shear Modulus  4.69 GPa
@Temperature 121 °C
680 ksi
@Temperature 250 °F
In-Plane, Wet; 270°F Oven Cure, 350°F Postcure; ASTM D3518
 4.76 GPa
@Temperature 23.9 °C
690 ksi
@Temperature 75.0 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
 4.83 GPa
@Temperature 121 °C
700 ksi
@Temperature 250 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
Shear Strength  79.3 MPa
@Temperature 121 °C
11500 psi
@Temperature 250 °F
In-Plane, Wet; 270°F Oven Cure, 350°F Postcure; ASTM D3518
 91.7 MPa
@Temperature 121 °C
13300 psi
@Temperature 250 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
 97.2 MPa
@Temperature 23.9 °C
14100 psi
@Temperature 75.0 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fabric Area Weight (g/m²)378270°F Oven Cure, 350°F Postcure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Solvay EF1812 Polycarbosilane Polymer, Pyrolized with T300 Carbon Fabric
Solvay LTM® 26EL Epoxy with T300 Woven Carbon Fiber Laminate
Park Aerospace Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber

PPARK018 / 89290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.