MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products MB 8250 Aluminum Board
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: MB 8250 is an aluminum filled product that is dimensionally stable and exhibits great machinable properties. Features: excellent machineability, low dust emission, no shrinkage, low moisture absorption, excellent surface detail reproduction, and excellent surface finish. Uses: proofing intricate NC designs, numerous tooling aids, master models (automotive/aerospace), various prototypes, architectural models, foundry applications, bases for Die models, and short run vacuum forming tools (low temperature).

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Tensile Strength, Ultimate 27.901 MPa4046.7 psi
Tensile Modulus 5.434 GPa788.2 ksi
Flexural Strength 46.655 MPa6766.7 psi
Flexural Modulus 4.221 GPa612.2 ksi
Compressive Strength 58.231 MPa8445.7 psi
Compressive Modulus 0.0924 GPa13.4 ksi
Izod Impact, Notched 0.726 J/cm1.36 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.6 µm/m-°C39.2 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU) (Extended Aging Data)
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Lubrizol LifeSciences Tecothane® TT-2075D-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecoplast® Series TP-470/Clear Resins TPU

PBCC016 / 107243

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.