MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded; Polyurethane, TP

Material Notes:
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Linear Mold Shrinkage  0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
48 hr at 80°C; ASTM D955
 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
72 hr; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Hardness, Shore D 757515 sec delay; ASTM D2240
Tensile Strength, Ultimate 55.0 MPa7980 psiat max load; ASTM D638
Elongation at Break 100 %100 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Flexural Modulus 2.30 GPa334 ksitangent; ASTM D790
Izod Impact, Notched 0.170 J/cm0.318 ft-lb/inASTM D256
 0.0400 J/cm
@Temperature -40.0 °C
0.0749 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.0500 J/cm
@Temperature 0.000 °C
0.0937 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
@Thickness 3.20 mm
185 °F
@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 3.20 mm
167 °F
@Thickness 0.126 in
ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU)
Lubrizol LifeSciences Tecoplast® Series TP-470/Clear Resins TPU
BCC Products MB 3500 Urethane Fixture Board
Miracll E175DL Thermoplastic Polyurethane (TPUR), Polyester Grade
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound

PASHU276 / 25240

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.