MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade

Processing and Delivery Form: Pellets and Injection Molding

Additives: Carbon fiber

Special Characteristics: High strength, Chemically resistant, High temp resistance

Information provided by Oxford Polymers

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ASTM D792
Water Absorption at Saturation 0.25 %0.25 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.17 mm
0.0020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 238 MPa34500 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 338 MPa49000 psiASTM D790
Flexural Modulus 19.48 GPa2825 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 343 °C650 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 343 - 360 °C650 - 680 °F
Middle Barrel Temperature 349 - 366 °C660 - 690 °F
Front Barrel Temperature 354 - 377 °C670 - 710 °F
Nozzle Temperature 357 - 382 °C675 - 720 °F
Melt Temperature 354 - 371 °C670 - 700 °F
Mold Temperature 177 - 199 °C350 - 390 °F
Drying Temperature <= 149 °C<= 300 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Oxford Polymers PC 714-FR Series PC, Flame retardant
VICTREX™ PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Oxford Polymers 604-I Polycarbonate/ABS Alloy

POXF014 / 178444

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.