MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group UV-408 Low-Viscosity, High Clarity, UV Curable Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: UV 408 is a low viscosity, high clarity, UV curing adhesive with excellent adhesion to glass. The product is well suited for bonding close fitting parts and has excellent moisture resistance.

Applications:

Lens bonding, Glass assembly, Fiber optic bonding.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 50 - 100 cP
@Temperature 25.0 °C
50 - 100 cP
@Temperature 77.0 °F
Uncured
Thickness <= 6350 microns<= 250 milCured film
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8787Cured
Tensile Strength at Break 46.9 MPa6800 psiCured
Elongation at Break 10 %10 %Cured
 
Thermal PropertiesMetricEnglishComments
CTE, linear 166 µm/m-°C
@Temperature 20.0 °C
92.2 µin/in-°F
@Temperature 68.0 °F
Cured
Flash Point >= 93.3 °C>= 200 °FUncured
Shrinkage 8.0 %8.0 %Upon cure
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %Mfr. Specifies clear but does not quantify
 
Descriptive Properties
ColorClear
CompositionUrethane Oligomer/ (Meth) Acrylate
SolubilityIsopropyl Alcohol, Chlorinated solvents
ToxicityLow
Water Resistance4 hoursCured, 1/4" x 1/4", boiling water, substrate failure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System
Resin Technology Group EN 239-2 Millennium™ UV Curable Adhesive
Resin Technology Group DPE111798-1 UV Curable Adhesive
Resin Technology Group UV-S-2051 High Impact, UV Curable Plastic Bonder
Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive

PRESINT643 / 65527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.