MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Master Bond UV15DC80 is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curing areas on parts that do not allow UV light curing because of “shadowing” issues. Most noteworthy is that the heat cure portion can be initiated at only 80°C rather than at the more common 125°C.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 50000 - 70000 cP50000 - 70000 cPuncured coating
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 70>= 70
Tensile Strength >= 34.5 MPa>= 5000 psi
Tensile Modulus >= 2.41 GPa>= 350 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.49
@Frequency 60 Hz
3.49
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 - 65.0 µm/m-°C30.6 - 36.1 µin/in-°F
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg >= 125 °C>= 257 °Fwith post cure
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.521.52
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Monthin original unopened containers
 
Descriptive Properties
Chemical ResistanceWater<1% weight gain, 30 month immersion, 75°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting

PMASTB276 / 132873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.