MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis LE4217 Polyethylene Compound, Crosslinkable, Track Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE4217 is a black crosslinkable polyethylene compound designed for track resistant power cable insulation and jacketing. APPLICATION: LE4217 contains carbon black and UV stabilizer and specifically suited for outdoor installations such as OC cables. LE4217 is suitable as a jacket or insulation, for power cables rated up to 35kV. However it is recommended that for cables rated above 12kV, that a suitable conductor shield such as LE0594 or LE0595 be used for optimum performance. Specifications: ICEA S-94-649.

Information provided by Borealis AG

Key Words: XLPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³base resin; ASTM D2839
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 300 %>= 300 %after aging 500h, 150°C; ASTM D638
 >= 360 %>= 360 %after xenon aging 2000h, 23°C; ASTM D2565
 400 %400 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmASTM D257
Dielectric Breakdown >= 3500 V>= 3500 VTracking Resistance; ASTM D2303
Dissipation Factor 0.00020
@Frequency 60000 Hz
0.00020
@Frequency 60000 Hz
ASTM D150
Track Resistance >= 1.08e+6 sec>= 1.08e+6 secASTM D2132
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Polycure™ PC531 Track Resistant Crosslinking Polyethylene Compound for Overhead Cable Insulation
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4244R Polyethylene Insulation Compound, Crosslinkable
Borealis LE4212L Polyethylene Insulation Compound, Crosslinkable
Avient Syncure™ S1006B Polyethylene, Crosslinked (XLPE)

PBOREA517 / 108776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.