MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics THERM-A-GAP™ GEL T630 Dispensable, Very Low Compression Force, Thermal Gap Filler
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance. These unique materials result in much lower mechanical stress on delicate components than even the softest gap-filling sheets. They are ideal for filling variable gaps between multiple components and a common heat sink.

Features/Benefits: Dispensable; Fully cured; Highly conformable at low pressures; No refrigeration, mixing or filler settling issues in storage; Single dispensable TIM can eliminate multiple pad part sizes/numbers; RoHS Compliant and Reworkable

Typical Applications: Automotive electronic control unites (ECUs), engine control, transmission control, braking/traction control; Power conversion equipment; Power supplies and uninterruptible power supplies; Power semiconductors; MOSFET arrays with common heat sinks and Televisions and consumer electronics.

Product Attributes: Years of proven reliability in high-volume automotive applications; General use material; Good thermal performance; Lowest deflection force required and Minimal stress on components

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.25 g/cc2.25 g/ccASTM D792
Thickness 100 microns3.94 milBondline
Deformation  36 %
@Thickness 2.54 mm,
Pressure 0.00689 MPa
36 %
@Thickness 0.100 in,
Pressure 1.00 psi
Dispensed 1.0 cc of material Brought 1" x 1" probe, Test rate 0.025 in/min; Modified ASTM C165
 47 %
@Thickness 2.54 mm,
Pressure 0.0138 MPa
47 %
@Thickness 0.100 in,
Pressure 2.00 psi
Dispensed 1.0 cc of material Brought 1" x 1" probe, Test rate 0.025 in/min; Modified ASTM C165
 54 %
@Thickness 2.54 mm,
Pressure 0.0207 MPa
54 %
@Thickness 0.100 in,
Pressure 3.00 psi
Dispensed 1.0 cc of material Brought 1" x 1" probe, Test rate 0.025 in/min; Modified ASTM C165
 59 %
@Thickness 2.54 mm,
Pressure 0.0276 MPa
59 %
@Thickness 0.100 in,
Pressure 4.00 psi
Dispensed 1.0 cc of material Brought 1" x 1" probe, Test rate 0.025 in/min; Modified ASTM C165
 63 %
@Thickness 2.54 mm,
Pressure 0.0345 MPa
63 %
@Thickness 0.100 in,
Pressure 5.00 psi
Dispensed 1.0 cc of material Brought 1" x 1" probe, Test rate 0.025 in/min; Modified ASTM C165
Outgassing - Total Mass Loss 0.55 %0.55 %ASTM E595
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Constant 5.5
@Frequency 1e+6 Hz
5.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 5.00 kV/mm127 kV/inASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Chomerics
 
Thermal PropertiesMetricEnglishComments
CTE, linear 350 µm/m-°C194 µin/in-°FASTM E831
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°FASTM D1269
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°FASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 MonthFrom date of manufacture; Chomerics
 
Descriptive Properties
ColorWhite
Flow Rate10 cc/min30cc taper tip, 0.13" orifice, 90 psi; Chomerics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics THERM-A-GAP™ GEL 30 High Performance Fully Cured Dispensable Gel
Parker Chomerics THERM-A-GAP™ GEL T630G Dispensable, Very Low Compression Force, Thermal Gap Filler
Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel
Parker Chomerics THERM-A-GAP™ GEL T635 Dispensable, Very Low Compression Force, Thermal Gap Filler
Parker Chomerics THERM-A-GAP™ GEL T636 Dispensable, Very Low Compression Force, Thermal Gap Filler

PCHOME299 / 131009

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.