MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics THERM-A-GAP™ GEL 8010 High Performance Fully Cured Dispensable Gel
Categories: Fluid

Material Notes: Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) complexity. These products require no mixing or curing, providing superior design flexibility. Provides low thermal impedance at thin and thick gaps, allowing use of common heat spreaders; Lower temperature increases product life, typically a doubling of life based on every 10°C decrease in temperature; Deflects easily under very low compressive forces, decreasing stress on components thus decreasing component failures.

Typical Applications: Automotive Electronic Control Units (ECU’s), Power Supplies & Semiconductors, Memory & Power Modules, Microprocessors/Graphics Processors, and Flat Panel Displays & Consumer Electronics.

Features/Benefits: Easily dispensable, Fully-cured/No pump out, High bulk thermal conductivity, Low thermal impedance, Ultra low compression force, High tack surface & reworkable and Proven long-term reliability.

Product Attributes: Thin bondline gel (approximately 2-10 mils), Low thermal impedance gel, Stencil printable with no pump out, Ideal for high-volume dispensing, and Proven long-term reliability.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.70 g/cc2.70 g/ccASTM D792
Thickness >= 50.0 microns>= 1.97 milBondline thickness
Deformation  27 %
@Pressure 0.00345 MPa
27 %
@Pressure 0.500 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
 45 %
@Pressure 0.00689 MPa
45 %
@Pressure 1.00 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
 52 %
@Pressure 0.0103 MPa
52 %
@Pressure 1.50 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
 57 %
@Pressure 0.0138 MPa
57 %
@Pressure 2.00 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
 60 %
@Pressure 0.0172 MPa
60 %
@Pressure 2.50 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
 63 %
@Pressure 0.0207 MPa
63 %
@Pressure 3.00 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
 65 %
@Pressure 0.0241 MPa
65 %
@Pressure 3.50 psi
Dispensed 1.0 cc of material, Brought 1" x 1" probe down to 0.1"; Test rate 0.025 in/min; Modified ASTM C165
Outgassing - Total Mass Loss 1.33 %1.33 %TML; ASTM E595
Collected Volatile Condensable Material 0.34 %0.34 %ASTM E595
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Constant 6.3
@Frequency 1e+6 Hz
6.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 8.00 kV/mm203 kV/inASTM D149
Dissipation Factor 0.0020
@Frequency 100000 Hz
0.0020
@Frequency 100000 Hz
Chomerics
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C83.3 µin/in-°FASTM E831
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°FASTM E1269
Thermal Conductivity 3.00 W/m-K20.8 BTU-in/hr-ft²-°FASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 MonthFrom date of Manufacture
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics THERM-A-GAP™ GEL 30 High Performance Fully Cured Dispensable Gel
Parker Chomerics THERM-A-GAP™ GEL T630 Dispensable, Very Low Compression Force, Thermal Gap Filler
Parker Chomerics THERM-A-GAP™ GEL T630G Dispensable, Very Low Compression Force, Thermal Gap Filler
Parker Chomerics THERM-A-GAP™ GEL T635 Dispensable, Very Low Compression Force, Thermal Gap Filler
Parker Chomerics THERM-A-GAP™ GEL T636 Dispensable, Very Low Compression Force, Thermal Gap Filler

PCHOME297 / 131007

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.