MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Seals Eastern 5862 Fluoro-silicone
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Fluoro-silicone

Information provided by Seals Eastern, Inc.

Key Words: FVMQ
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 53>= 53ASTM D2240, Type A
 6161AVG; ASTM D2240, Type A
Tensile Strength at Break >= 11.0 MPa>= 1590 psiASTM D412 Method A
 11.2 MPa1630 psiAVG; ASTM D412 Method A
Tensile Stress at Strain  0.965 MPa
@Strain 25 %
140 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 1.38 MPa
@Strain 50 %
>= 200 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 1.49 MPa
@Strain 50 %
216 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 2.45 MPa
@Strain 100 %
>= 356 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 2.54 MPa
@Strain 100 %
369 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 320 %>= 320 %ASTM D412 Method A
 325 %325 %AVG; ASTM D412 Method A
Modulus of Elasticity 0.00528 GPa0.766 ksiASTM D412 Method A
Poissons Ratio 0.370.37Calculated
Shear Modulus 0.00193 GPa0.280 ksiASTM D412 Method A
Secant Modulus 0.00512 GPa0.743 ksiASTM D412 Method A
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -51.1 °C-60.0 °FASTM D1329
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 5861 Fluoro-silicone
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Seals Eastern 5803 Fluoro-silicone
Freudenberg S310 Silicone Elastomer (VMQ)
Freudenberg S315 Silicone Elastomer (VMQ)

PSEAL45 / 80192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.