MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Seals Eastern 5803 Fluoro-silicone
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Fluoro-silicone

Information provided by Seals Eastern, Inc.

Key Words: FVMQ
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 70>= 70ASTM D2240, Type A
 7575AVG; ASTM D2240, Type A
Tensile Strength at Break >= 6.936 MPa>= 1006 psiASTM D412 Method A
 7.143 MPa1036 psiAVG; ASTM D412 Method A
Tensile Stress at Strain  1.51 MPa
@Strain 25 %
219 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 2.36 MPa
@Strain 50 %
>= 343 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 2.45 MPa
@Strain 50 %
356 psi
@Strain 50 %
Average; ASTM D412 Method A
 >= 4.48 MPa
@Strain 100 %
>= 650 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 4.57 MPa
@Strain 100 %
663 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 172 %>= 172 %ASTM D412 Method A
 182 %182 %AVG; ASTM D412 Method A
Modulus of Elasticity 0.0112 GPa1.62 ksiASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.00372 GPa0.540 ksiASTM D412 Method A
Secant Modulus 0.01016 GPa1.473 ksiASTM D412 Method A
Compression Set 19 %
@Temperature 150 °C,
Time 79200 sec
19 %
@Temperature 302 °F,
Time 22.0 hour
ASTM D395, Test B
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)29

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 5861 Fluoro-silicone
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Seals Eastern 5862 Fluoro-silicone
Freudenberg S60 Silicone Elastomer (VMQ)
ATG s.r.l. FVMQ Fluorosilicone Rubber

PSEAL44 / 80191

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.