MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 3 Part Heat Treatment, 8.0 inch (203 mm) Diameter
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Iron Base

Material Notes: Tensile strength (ultimate and yield), compressive strength, reduction of area, and elongation values reported here are typical for Hot Finished Rod, 3 Part Heat Treatment, 8.0 inch (203 mm) Diameter samples. Density and magnetic permeability are typical of precipitation hardened INCONEL® alloy 706. Other property values are typical of INCONEL® alloy 706.

For optimum creep and rupture properties, the alloy receives a three part heat treatment as follows: Solution treat 1700-1850°F (925-1010°C) for a time commensurate with section size, then air cool. Stabilizing treatment 1550°F (845°C)/3 hr, air cool. Precipitation treatment 1325°F (720°C)/8 hr, furnace cool at 100°F (55°C)/hr to 1150°F (620°C)/8 hr, air cool.

Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.08 g/cc0.292 lb/in³Precipitation Hardened
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1300 MPa189000 psi
Tensile Strength, Yield 1010 MPa
@Strain 0.2 %
146000 psi
@Strain 0.2 %
Elongation at Break 18 %18 %
Reduction of Area 28 %28 %
Modulus of Elasticity 210 GPa30500 ksiDynamic Method
Compressive Yield Strength 1102 MPa159900 psi(0.2% Offset) Thickness not reported for this value
Poissons Ratio 0.3820.382Calculated by mfr.
Shear Modulus 76.0 GPa11000 ksiDynamic Method
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000985 ohm-cm0.0000985 ohm-cm
Magnetic Permeability 1.011.01at 200 Oersted (15.9 kA/m); Annealed
Curie Temperature <= -78.0 °C<= -108 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.46 µm/m-°C
@Temperature 24.0 - 100 °C
7.478 µin/in-°F
@Temperature 75.2 - 212 °F
Mean
 15.08 µm/m-°C
@Temperature 24.0 - 300 °C
8.378 µin/in-°F
@Temperature 75.2 - 572 °F
Mean
 15.59 µm/m-°C
@Temperature 24.0 - 500 °C
8.661 µin/in-°F
@Temperature 75.2 - 932 °F
Mean
 16.42 µm/m-°C
@Temperature 21.0 - 700 °C
9.122 µin/in-°F
@Temperature 69.8 - 1290 °F
Mean
Specific Heat Capacity 0.444 J/g-°C0.106 BTU/lb-°F
Thermal Conductivity 12.5 W/m-K86.8 BTU-in/hr-ft²-°F
Melting Point 1334 - 1371 °C2433 - 2500 °F
Solidus 1334 °C2433 °F
Liquidus 1371 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.060 %<= 0.060 %
Boron, B <= 0.0060 %<= 0.0060 %
Carbon, C <= 0.30 %<= 0.30 %
Chromium, Cr 14.5 - 17.5 %14.5 - 17.5 %
Cobalt, Co <= 1.0 %<= 1.0 %
Copper, Cu <= 0.35 %<= 0.35 %
Iron, Fe 38 %38 %As remainder
Manganese, Mn <= 0.35 %<= 0.35 %
Nickel, Ni 39 - 44 %39 - 44 %Including Cobalt
Niobium, Nb (Columbium, Cb) 2.5 - 3.3 %2.5 - 3.3 %Includes Ta
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.35 %<= 0.35 %
Sulfur, S <= 0.015 %<= 0.015 %
Titanium, Ti <= 0.40 %<= 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
Titanium Ti-6Al-4V (Grade 5), Annealed
Special Metals INCONEL® Alloy 718
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)

NINCO48 / 17481

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.