MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Nickel Alloy; Superalloy

Material Notes: Data provided by Carpenter Technology Corporation.

Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ductility and toughness, and excellent corrosion resistance. In addition, this alloy displays exceptional resistance to sulfidation, high temperature oxidation, and hydrogen embrittlement. The unique properties of MP35N alloy are developed through work hardening, phase transformation and aging. If the alloy is used in the fully work hardened condition, service temperatures up to 750°F (399°C) are suggested. MP35N alloy is normally produced by vacuum induction melting (VIM), followed vacuum arc remelting (VAR).

Because of its unique combination of properties, MP35N alloy has been used in a wide variety of applications. MP35N alloy has been used in fasteners, springs, nonmagnetic electrical components and instrument parts in medical, seawater, oil and gas well, and chemical and food processing environments.

*MP35N is a trademark of SPS Technologies, Inc. MP is a registered trademark of SPS Technologies, Inc.

Key Words: UNS R30035; AMS 5758; AMS 5844; AMS 5845; ANSI F562; ASTM F562
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.43 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2027 MPa294000 psi
 1655 MPa
@Temperature 426 °C
240000 psi
@Temperature 799 °F
 1689 MPa
@Temperature 371 °C
245000 psi
@Temperature 700 °F
 1724 MPa
@Temperature 316 °C
250000 psi
@Temperature 601 °F
 1744 MPa
@Temperature 260 °C
252900 psi
@Temperature 500 °F
 1793 MPa
@Temperature 204 °C
260100 psi
@Temperature 399 °F
 1834 MPa
@Temperature 149 °C
266000 psi
@Temperature 300 °F
Tensile Strength, Yield 1965 MPa
@Strain 0.2 %
285000 psi
@Strain 0.2 %
 1551 MPa
@Strain 0.2 %,
Temperature 426 °C
225000 psi
@Strain 0.2 %,
Temperature 799 °F
 1586 MPa
@Strain 0.2 %,
Temperature 371 °C
230000 psi
@Strain 0.2 %,
Temperature 700 °F
 1627 MPa
@Strain 0.2 %,
Temperature 316 °C
236000 psi
@Strain 0.2 %,
Temperature 601 °F
 1662 MPa
@Strain 0.2 %,
Temperature 260 °C
241100 psi
@Strain 0.2 %,
Temperature 500 °F
 1710 MPa
@Strain 0.2 %,
Temperature 204 °C
248000 psi
@Strain 0.2 %,
Temperature 399 °F
 1758 MPa
@Strain 0.2 %,
Temperature 149 °C
255000 psi
@Strain 0.2 %,
Temperature 300 °F
Elongation at Break 10 %10 %
 4.0 %
@Temperature 426 °C
4.0 %
@Temperature 799 °F
 7.0 %
@Temperature 371 °C
7.0 %
@Temperature 700 °F
 8.0 %
@Temperature 149 °C
8.0 %
@Temperature 300 °F
 8.0 %
@Temperature 316 °C
8.0 %
@Temperature 601 °F
 8.0 %
@Temperature 260 °C
8.0 %
@Temperature 500 °F
 8.0 %
@Temperature 204 °C
8.0 %
@Temperature 399 °F
Reduction of Area 46 %46 %
 8.0 %
@Temperature 426 °C
8.0 %
@Temperature 799 °F
 22 %
@Temperature 371 °C
22 %
@Temperature 700 °F
 41 %
@Temperature 316 °C
41 %
@Temperature 601 °F
 43 %
@Temperature 260 °C
43 %
@Temperature 500 °F
 44 %
@Temperature 204 °C
44 %
@Temperature 399 °F
 45 %
@Temperature 149 °C
45 %
@Temperature 300 °F
Modulus of Elasticity 234.8 GPa34060 ksi
Poissons Ratio 0.450.45Calculated
Shear Modulus 80.95 GPa11740 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0001033 ohm-cm
@Temperature 23.0 °C
0.0001033 ohm-cm
@Temperature 73.4 °F
 0.0001154 ohm-cm
@Temperature 538 °C
0.0001154 ohm-cm
@Temperature 1000 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.8 µm/m-°C
@Temperature 21.0 - 93.0 °C
7.11 µin/in-°F
@Temperature 69.8 - 199 °F
 14.8 µm/m-°C
@Temperature 21.0 - 316 °C
8.22 µin/in-°F
@Temperature 69.8 - 601 °F
 15.7 µm/m-°C
@Temperature 21.0 - 538 °C
8.72 µin/in-°F
@Temperature 69.8 - 1000 °F
Thermal Conductivity  11.2 W/m-K
@Temperature 23.0 °C
77.7 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
 17.0 W/m-K
@Temperature 316 °C
118 BTU-in/hr-ft²-°F
@Temperature 601 °F
 23.4 W/m-K
@Temperature 649 °C
162 BTU-in/hr-ft²-°F
@Temperature 1200 °F
Melting Point 1315 - 1440 °C2399 - 2620 °F
Solidus 1315 °C2399 °F
Liquidus 1440 °C2620 °F
Maximum Service Temperature, Air 399 °C750 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.010 %0.010 %
Carbon, C <= 0.025 %<= 0.025 %
Chromium, Cr 19 - 21 %19 - 21 %
Cobalt, Co 33 %33 %as remainder
Iron, Fe <= 1.0 %<= 1.0 %
Manganese, Mn <= 0.15 %<= 0.15 %
Molybdenum, Mo 9.0 - 10.5 %9.0 - 10.5 %
Nickel, Ni 33 - 37 %33 - 37 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.15 %<= 0.15 %
Sulfur, S <= 0.010 %<= 0.010 %
Titanium, Ti <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 53% Cold Reduction + Aged 538°C (1000°F)/4hr/AC
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction
Titanium Ti-6Al-4V (Grade 5), Annealed

NCARCK / 15740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.