MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal KLINGERSIL® C-4408 Metal Reinforced Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Synthetic Fiber
  • Nitrile Binder
  • High Temperature & Stress
  • Fluctuating Temperatures & Pressures
  • Vibration
  • Low Carbon Steel Woven Mesh Insert

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ASTM F1315
Thickness 1588 microns62.52 milThickness tested
 
Descriptive Properties
ColorBlack(Top/Bottom)
Compressibility8 percentASTM F36J
Creep Relaxation20 percent1/32", ASTM F38B
Klinger Hot Compression Test10 percentInitial, Thickness Decrease 73°F (23°C)
 22 percentAdditional, Thickness Decrease 572°F (300°C)
Recovery>50 percentASTM F36J
Thickness Increase0-5%ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
 0-5%ASTM Oil IRM903, 5h/300°F (149°C)
 0-5%ASTM Fuel A, 5h/73°F (23°C)
 0-5%ASTM Fuel B, 5h/73°F (23°C)
Weight Increase<10%ASTM F146 after immersion in Fuel B 5h/73°F (23°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Klinger Thermoseal KLINGERSIL® C-4401 General Application Gasketing
RTP Company RTP 4408 L High Temperature Nylon (HTN), Glass Fiber - Lubricated
RTP Company RTP 4408 HS L High Temperature Nylon (HTN), Glass Fiber - Heat Stabilized - Lubricated
Parker Chomerics CHO-FLEX 4408 Conductive Ink
Garlock GYLON® HP3561 PTFE Gasketing, Steel Insert

PTHERM909 / 146062

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.