MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal KLINGERSIL® C-4401 General Application Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Synthetic Fiber
  • Nitrile Binder
  • Excellent Sealability
  • Excellent Chemical Resistance
  • Good Creep Relaxation
  • General Purpose Sheet

Data for this material is available for download into ANSYS xml format: C4401; 1/64" (right click and "save as" to download)

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ASTM F1315
Thickness 1588 microns62.52 milThickness tested
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.0 kV/mm356 kV/inASTM D149-95a
 
Descriptive Properties
ColorGreen(Top/Bottom)
Compressibility7 percentASTM F36J
Creep Relaxation20 percent1/32", ASTM F38B
Gas Permeability<0.5 ml/minDIN 3535/6
Klinger Hot Compression Test10.5 percentInitial, Thickness Decrease 73°F (23°C)
 17 percentAdditional, Thickness Decrease 572°F (300°C)
Leachable Chloride Content100 ppmFSA Method (Typical)
Recovery>50 percentASTM F36J
Sealability<0.25 ml/hr1/32", ASTM F37A
Thickness Increase0-5%ASTM F146 after immersion in ASTM Oil 1, 5h/300°F (149°C)
 0-5%ASTM Oil IRM903, 5h/300°F (149°C)
 0-5%ASTM Fuel A, 5h/73°F (23°C)
 0-7%ASTM Fuel B, 5h/73°F (23°C)
Weight Increase<10%ASTM F146 after immersion in Fuel B 5h/73°F (23°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Klinger Thermoseal ML-5270 PTG Gasketing
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Special Metals INCONEL® Alloy 625
Polimersan Plastics POLIPOM® (POM)

PTHERM908 / 146061

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.