MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 216 V45 PA6, 45% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Description: Polyamide PA6, reinforced with 45% of glass fiber, for injection molding.

Available in: Europe

Product Applications: TECHNYL C 216 V45 has been optimized to have high impact strength, a nice surface aspect and being easy to paint. It has been especially developed for the market of ski bindings, but can be advised as well for any part requiring a high rigidity as well as high impact strength. This product is available in natural and black colors

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
0.80 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiISO 527 Type 1A
Elongation at Break 2.5 %2.5 %ISO 527 Type 1A
Tensile Modulus 13.0 GPa1890 ksiISO 527 Type 1A
Charpy Impact Unnotched 9.00 J/cm²42.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 475 V475 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75/Af
 
Processing PropertiesMetricEnglishComments
Feed Temperature 225 - 230 °C437 - 446 °F
Front Barrel Temperature 245 - 255 °C473 - 491 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone240-255°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Domo TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Domo TECHNYL® C 216 V45 PA6, 45% glass fiber, Conditioned
Domo TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0

PRHOD761 / 137992

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.