MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled

Material Notes: Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.

Applications:

  • Firearms
  • Automotive
  • Household appliances

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Filler Content 10 %10 %ASTM D2584
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 1.59 mm
0.0030 in/in
@Thickness 0.0625 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength at Break 65.5 MPa9500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 4.62 GPa670 ksiASTM D638
Flexural Strength 102 MPa14800 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiTangent; ASTM D790
Compressive Strength 82.7 MPa12000 psiASTM D695
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inAt 73°F; ASTM D256
Izod Impact, Unnotched 2.99 J/cm5.60 ft-lb/inAt 73°F; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.0
@Frequency 10000 Hz
3.0
@Frequency 10000 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm450 kV/inASTM D149
Dissipation Factor 0.0080
@Frequency 10000 Hz
0.0080
@Frequency 10000 Hz
ASTM D150
Arc Resistance 80 sec80 secDry; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C
@Temperature 20.0 °C
12.8 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 60.0 °C140 °FContinuous use; UL 746B
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.8 °C208 °FASTM D648
Flammability, UL94 HBHBClass 1/16
Oxygen Index <= 27 %<= 27 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled

PPOLI035 / 56939

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.