MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo INSPIRE™ TF1500 ESU Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Talc filled, high impact PP compound. INSPIRE™ TF1500 ESU has been developed for aesthetic automotive applications, with good scratch resistance and UV light stabilization. It is especially suitable for car interior applications requiring ductility, because of its high impact resistance, even at low temperatures.

Application areas:

  • Instrument panel retainer
  • Instrument panel trim
  • Midconsole
  • Door panels
  • Door pockets
  • Interior trim
  • Trunk trim
Automotive Specifications:
  • GM QK 004022 U Color: Charcoal
  • PSA Peugeot-Citroen SPA 3858
  • IMDS ID 21758150 Color: Charcoal
Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Filler Content 15 %15 %Talc
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psi50mm/min; ISO 527
Elongation at Break 70 %70 %50 mm/min; ISO 527
Tensile Modulus 1.95 GPa283 ksi1 mm/min; ISO 527
Flexural Modulus 1.85 GPa268 ksi3 points and 2 mm/min; ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²11.9 ft-lb/in²ISO 180/1A
 5.00 kJ/m²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 10.0 kJ/m²
@Temperature 0.000 °C
4.76 ft-lb/in²
@Temperature 32.0 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 85.0 µm/m-°C
@Temperature 20.0 °C
47.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FUnannealed; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °FUnannealed; ISO 75
Vicat Softening Point 135 °C275 °FISO 306 A
Shrinkage 0.90 - 1.2 %0.90 - 1.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® T85 XF Polycarbonate + ABS
Trinseo Magnum™ 3416 SC Natural Plus ABS Resin
Trinseo PULSE™ 920 MG PC/ABS
Trinseo PULSE™ A35-105 PC/ABS
Borealis Daplen™ EE188HP Polypropylene TPO Compound

PZZDOW1148 / 30352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.