MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchcast™ 5230N Electrical Epoxy Powder Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: 3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a variety of substrates. Scotchcast 5230N is manufactured by a fusion blend process, insuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Scotchcast 5230 is applied to a cold object via the electrostatic fluid bed process. The negatively charged resin particles are attracted to the grounded object to be coated. Coating thicknesses up to 25 mils may be obtained. Because of its superior charging capabilities Scotchast 5230N exhibits excellent slot penetration on motor stators and armatures. Uses for Scotchcast 5230N include moisture-proofing and insulating armatures, stator, buss bars and toroid cores.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³cured; ASTM D794
 
Mechanical PropertiesMetricEnglishComments
Gardner Impact 18.1 J13.3 ft-lb12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Abrasion 0.110.11[g]; ASMT D4060
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 39.4 kV/mm1000 kV/in12 to 15 mil coating; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FASTM E1530
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Temperature 232 °C
0.0500 hour
@Temperature 450 °F
 6.00 min
@Temperature 204 °C
0.100 hour
@Temperature 399 °F
 15.0 min
@Temperature 177 °C
0.250 hour
@Temperature 351 °F
Gel Time 0.150 - 0.640 min
@Temperature 193 °C
0.150 - 0.640 min
@Temperature 379 °F
hot plate
Shelf Life 24.0 Month
@Temperature <=16.0 °C
24.0 Month
@Temperature <=60.8 °F
 
Descriptive Properties
AppearanceBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin
Master Bond EP21SC-1 Two Component Epoxy Resin System
3M Scotchcast™ 5555 22G Electrical Insulating Epoxy Resin
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin
3M Scotchcast™ 265 Electrical Epoxy Powder Resin

PMM35355 / 170102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.