MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchcast™ 5555 22G Electrical Insulating Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating for motor stators, armatures, and transformers. Electrical resin 5555 is manufactured by a fusion blend process, insuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Resin 5555 can be applied via cold electrostatic fluid bed, hot venture spray or hot fluid bed dip. When applied electrostacially to a cold part, induction heat is recommended to melt and flow the powder to a tough, moisture and chemical resistant dielectric coating for various electrical devices. When applied to a hot part the resin melts, flows to a controlled extent, the cures, bonding to the substrate and coalescing into a smooth, continuous, essentially uniform, thick dielectric coating. Resin 5555 has two gel times in order to accommodate those applications that need slightly higher flow, or for application equipment that requires rapid curing.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³cured; ASTM D794
 
Mechanical PropertiesMetricEnglishComments
Gardner Impact 11.3 J8.33 ft-lb12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 51.2 kV/mm1300 kV/in12 to 14 mil coating; ASTM D149
 
Processing PropertiesMetricEnglishComments
Cure Time  2.00 min
@Temperature 232 °C
0.0333 hour
@Temperature 450 °F
 4.00 min
@Temperature 204 °C
0.0667 hour
@Temperature 399 °F
 8.00 min
@Temperature 177 °C
0.133 hour
@Temperature 351 °F
Gel Time 0.350 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 193 °C
0.350 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min
@Temperature 379 °F
hot plate
Shelf Life 18.0 Month
@Temperature <=21.1 °C
18.0 Month
@Temperature <=70.0 °F
 
Descriptive Properties
AppearanceGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchcast™ 5230N Electrical Epoxy Powder Resin
3M Scotchcast™ 265 Electrical Epoxy Powder Resin
Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive
Master Bond EP21SC-1 Two Component Epoxy Resin System
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness

PMM35357 / 170104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.