MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion pan/frame to be made of an engineering plastic as opposed to metal. TG7S BK-102 exhibits improved strength, stiffness and notched impact properties over Ultramid 8333G HI.

Applications: Include cushion seat pan/frame and other automotive seating applications, automotive fan, power tools and trimmer components.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Melt Flow 18.15 g/10 min
@Load 5.00 kg,
Temperature 235 °C
18.15 g/10 min
@Load 11.0 lb,
Temperature 455 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psiISO 527
Elongation at Break 3.5 %3.5 %ISO 527
Flexural Modulus 4.42 GPa641 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FISO 75
 
Processing PropertiesMetricEnglishComments
Zone 1 245 - 275 °C473 - 527 °FRear Zone
Zone 2 260 - 285 °C500 - 545 °FCenter Zone
Zone 3 270 - 295 °C518 - 563 °FFront Zone
Zone 4 270 - 295 °C518 - 563 °FNozzle
Melt Temperature 270 - 295 °C518 - 563 °F
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.080 %<= 0.080 %
 
Descriptive Properties
ColorBK 5966
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Envalior Akulon® K223-TP4 PA6-I, Dry, Impact Modified
Avient Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6)

PBASG0428 / 132061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.