MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing enhanced surface appearance versus nylon 6/6 compounds. These materials are available in a broad range of reinforcement levels depending upon stiffness characteristics desired and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Filler Content 33 %33 %Glass Fiber Reinforcement
Water Absorption 0.81 %0.81 %24h/23C; ISO 62
 1.0 %
@Thickness 3.18 mm
1.0 %
@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 182 MPa26400 psiISO 527
Tensile Strength, Yield 165 MPa23900 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 12 %12 %ISO 527
Elongation at Yield 4.0 %4.0 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 241 MPa35000 psiASTM D790
 242 MPa35100 psiISO 178
Flexural Modulus 8.27 GPa1200 ksiASTM D790
 9.31 GPa1350 ksiISO 178
Izod Impact, Notched 1.30 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.44 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²Partial Break; ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
@Thickness 3.18 mm
428 °F
@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 202 °C396 °FAnnealed; ISO 75-2/A
 206 °C
@Thickness 3.18 mm
403 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 48.9 - 93.3 °C120 - 200 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AppearanceNatural Color
Automotive SpecificationsCHRYSLER MS-DB41 CPN2625 Color: 100% Color Match
 CHRYSLER MS-DB41 CPN4338 Color: Non-matched Color
FeaturesGeneral Purpose
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
Envalior Akulon® K223-TP4 PA6-I, Dry, Impact Modified
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Conditioned)
BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry)

PH0POL0025 / 144594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.