MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shakespeare MX-229 PVDF Monofilament
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Outstanding resistance to weathering/UV exposure; outstanding chemical resistance; low surface energy; low COF; low moisture regain; inherent flame resistance.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³
Fiber Count 2060 dtex1850 denier
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 5.5 %5.5 %
Tenacity 0.416 N/tex4.71 g/denier
 
Thermal PropertiesMetricEnglishComments
Melting Point 174 °C345 °F
Maximum Service Temperature, Air 150 °C302 °FContinuous Use
Shrinkage 9.13 %9.13 %Boiling Water/5 Min.
 16.3 %
@Temperature 132 °C,
Time 601 sec
16.3 %
@Temperature 270 °F,
Time 0.167 hour
Free Shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Griltech Grilon® BS 22R Nylon 6 Monofilament (Super-Set)
CHT Group QSil 229 Transparent, Liquid Silicone Rubber
Cast Stainless Steel CB7Cu-2, AMS 5400
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 55 HRC
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 45 HRC

PSHAKE228 / 67507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.