System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Shakespeare MX-229 PVDF Monofilament
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polyvinylidene Fluoride (PVDF)
;
Polyvinylidinefluoride (PVDF), Molded/Extruded
Material Notes:
Outstanding resistance to weathering/UV exposure; outstanding chemical resistance; low surface energy; low COF; low moisture regain; inherent flame resistance.
Information provided by Shakespeare Company.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.78
g/cc
Fiber Count
1850
denier
Mechanical Properties
Original Value
Comments
Elongation at Break
5.5 %
Tenacity
4.71
g/denier
Thermal Properties
Original Value
Comments
Melting Point
174
°C
Maximum Service Temperature, Air
150
°C
Continuous Use
Shrinkage
9.13 %
Boiling Water/5 Min.
16.3 %
@Temperature 132 °C,
Time 601 sec
Free Shrinkage
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
EMS-Griltech Grilon® BS 22R Nylon 6 Monofilament (Super-Set)
CHT Group QSil 229 Transparent, Liquid Silicone Rubber
Cast Stainless Steel CB7Cu-2, AMS 5400
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 55 HRC
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 45 HRC
PSHAKE228 / 67507
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.