MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 612, Unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.900 - 1.52 g/cc0.0325 - 0.0549 lb/in³Average value: 1.08 g/cc Grade Count:100
Water Absorption 0.200 - 3.00 %0.200 - 3.00 %Average value: 1.29 % Grade Count:60
Moisture Absorption at Equilibrium 0.500 - 3.00 %0.500 - 3.00 %Average value: 1.21 % Grade Count:31
Water Absorption at Saturation 1.60 - 9.00 %1.60 - 9.00 %Average value: 3.71 % Grade Count:56
Particle Size 5.00 - 30.0 µm5.00 - 30.0 µmAverage value: 17.0 µm Grade Count:3
Specific Surface Area 1.50 - 20.0 m²/g1.50 - 20.0 m²/gAverage value: 9.17 m²/g Grade Count:3
Water Vapor Transmission 15.1 - 20.2 g/m²/day0.970 - 1.30 g/100 in²/dayAverage value: 16.1 g/m²/day Grade Count:5
Oxygen Transmission 55.0 - 250 cc-mm/m²-24hr-atm140 - 635 cc-mil/100 in²-24hr-atmAverage value: 115 cc-mm/m²-24hr-atm Grade Count:5
Carbon Dioxide Transmission 200 - 850 cc-mm/m²-24hr-atm508 - 2160 cc-mil/100 in²-24hr-atmAverage value: 470 cc-mm/m²-24hr-atm Grade Count:5
Viscosity  50000 - 1.60e+6 cP
@Temperature 230 - 275 °C
50000 - 1.60e+6 cP
@Temperature 446 - 527 °F
Average value: 310000 cP Grade Count:3
 50000 - 1.60e+6 cP
@Shear Rate 30.0 - 8400 1/s
50000 - 1.60e+6 cP
@Shear Rate 30.0 - 8400 1/s
Average value: 310000 cP Grade Count:3
Viscosity Number 120 - 220 cm³/g1.20 - 2.20 dl/gAverage value: 165 cm³/g Grade Count:3
Thickness 10.0 - 25.0 microns0.394 - 0.984 milAverage value: 18.3 microns Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cm0.00100 - 0.0250 in/inAverage value: 0.0126 cm/cm Grade Count:50
Linear Mold Shrinkage, Transverse 0.00300 - 0.0300 cm/cm0.00300 - 0.0300 in/inAverage value: 0.0161 cm/cm Grade Count:39
Melt Flow 10.0 - 250 g/10 min10.0 - 250 g/10 minAverage value: 102 g/10 min Grade Count:9
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108 - 115108 - 115Average value: 114 Grade Count:7
Hardness, Shore D 68.0 - 82.068.0 - 82.0Average value: 76.4 Grade Count:7
Ball Indentation Hardness 30.0 - 220 MPa4350 - 31900 psiAverage value: 101 MPa Grade Count:19
Tensile Strength, Ultimate 31.0 - 185 MPa4500 - 26800 psiAverage value: 63.1 MPa Grade Count:30
Film Tensile Strength at Yield, MD 20.0 - 30.0 MPa2900 - 4350 psiAverage value: 27.6 MPa Grade Count:5
Film Tensile Strength at Yield, TD 18.0 - 30.0 MPa2610 - 4350 psiAverage value: 26.8 MPa Grade Count:5
Tensile Strength, Yield 26.0 - 66.0 MPa3770 - 9570 psiAverage value: 52.9 MPa Grade Count:55
Film Elongation at Break, MD 800 - 900 %800 - 900 %Average value: 840 % Grade Count:5
Film Elongation at Break, TD 900 %900 %Average value: 900 % Grade Count:5
Film Elongation at Yield, MD 4.30 - 15.0 %4.30 - 15.0 %Average value: 10.7 % Grade Count:6
Film Elongation at Yield, TD 8.00 - 15.0 %8.00 - 15.0 %Average value: 10.6 % Grade Count:5
Elongation at Break 0.000 - 303 %0.000 - 303 %Average value: 63.5 % Grade Count:76
Elongation at Yield 4.00 - 70.0 %4.00 - 70.0 %Average value: 12.9 % Grade Count:45
Modulus of Elasticity 0.350 - 15.5 GPa50.8 - 2250 ksiAverage value: 2.20 GPa Grade Count:86
 0.300 - 0.800 GPa
@Temperature 100 - 100 °C
43.5 - 116 ksi
@Temperature 212 - 212 °F
Average value: 0.500 GPa Grade Count:2
Flexural Yield Strength 30.0 - 1800 MPa4350 - 261000 psiAverage value: 136 MPa Grade Count:27
Flexural Modulus 0.750 - 2.76 GPa109 - 400 ksiAverage value: 1.98 GPa Grade Count:32
Izod Impact, Notched 0.320 - 1.07 J/cm0.600 - 2.00 ft-lb/inAverage value: 0.534 J/cm Grade Count:11
 0.500 - 0.500 J/cm
@Temperature -40.0 - -40.0 °C
0.937 - 0.937 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.500 J/cm Grade Count:1
Izod Impact, Unnotched 2.14 - 5340 J/cm4.00 - 10000 ft-lb/inAverage value: 4.27 J/cm Grade Count:4
Izod Impact, Notched (ISO) 3.30 - 12.0 kJ/m²1.57 - 5.70 ft-lb/in²Average value: 5.26 kJ/m² Grade Count:14
 3.00 - 7.10 kJ/m²
@Temperature -40.0 - -30.0 °C
1.43 - 3.38 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 4.42 kJ/m² Grade Count:10
Charpy Impact Unnotched 7.56 J/cm² - NB36.0 ft-lb/in² - NBAverage value: 8.24 J/cm² Grade Count:67
 2.00 J/cm² - NB
@Temperature -40.0 - -30.0 °C
9.52 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 6.67 J/cm² Grade Count:66
Charpy Impact, Notched 0.320 - 2100 J/cm²1.52 - 9990 ft-lb/in²Average value: 2.11 J/cm² Grade Count:73
 0.280 - 7.50 J/cm²
@Temperature -40.0 - -30.0 °C
1.33 - 35.7 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 0.931 J/cm² Grade Count:66
Tear Strength Test 371371Average value: 371 Grade Count:5
Elmendorf Tear Strength MD 2040 - 8160 g2040 - 8160 gAverage value: 4490 g Grade Count:5
Elmendorf Tear Strength TD 2040 - 8160 g2040 - 8160 gAverage value: 4490 g Grade Count:5
Film Tensile Strength at Break, MD 70.3 - 90.3 MPa10200 - 13100 psiAverage value: 81.1 MPa Grade Count:5
Film Tensile Strength at Break, TD 55.0 - 75.2 MPa7980 - 10900 psiAverage value: 67.1 MPa Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+15 ohm-cm1.00e+9 - 1.00e+15 ohm-cmAverage value: 1.45e+14 ohm-cm Grade Count:49
Surface Resistance 1.00e+10 - 1.00e+15 ohm1.00e+10 - 1.00e+15 ohmAverage value: 5.04e+13 ohm Grade Count:21
Dielectric Constant 2.90 - 12.02.90 - 12.0Average value: 4.04 Grade Count:20
Dielectric Strength 15.0 - 41.0 kV/mm381 - 1040 kV/inAverage value: 32.5 kV/mm Grade Count:49
Dissipation Factor 0.0140 - 0.1500.0140 - 0.150Average value: 0.0461 Grade Count:18
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:27
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.70 - 270 µm/m-°C0.944 - 150 µin/in-°FAverage value: 126 µm/m-°C Grade Count:32
 120 - 120 µm/m-°C
@Temperature 35.0 - 55.0 °C
66.7 - 66.7 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 120 µm/m-°C Grade Count:1
 120 - 120 µm/m-°C
@Thickness 2.00 - 2.00 mm
66.7 - 66.7 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 120 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 90.0 - 136 µm/m-°C50.0 - 75.6 µin/in-°FAverage value: 106 µm/m-°C Grade Count:17
Specific Heat Capacity 1.67 - 2.80 J/g-°C0.399 - 0.669 BTU/lb-°FAverage value: 2.15 J/g-°C Grade Count:5
Thermal Conductivity 0.180 - 0.280 W/m-K1.25 - 1.94 BTU-in/hr-ft²-°FAverage value: 0.233 W/m-K Grade Count:4
Melting Point 130 - 224 °C266 - 435 °FAverage value: 208 °C Grade Count:73
Maximum Service Temperature, Air 80.0 - 215 °C176 - 419 °FAverage value: 136 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 210 °C158 - 410 °FAverage value: 147 °C Grade Count:50
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 190 °C122 - 374 °FAverage value: 69.9 °C Grade Count:57
Vicat Softening Point 110 - 211 °C230 - 412 °FAverage value: 178 °C Grade Count:20
Minimum Service Temperature, Air -100 - -40.0 °C-148 - -40.0 °FAverage value: -55.0 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:43
 
Optical PropertiesMetricEnglishComments
Gloss 130 %130 %Average value: 130 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 279 °C374 - 535 °FAverage value: 226 °C Grade Count:3
Die Temperature 240 - 280 °C464 - 536 °FAverage value: 265 °C Grade Count:3
Melt Temperature 220 - 290 °C428 - 554 °FAverage value: 253 °C Grade Count:28
Mold Temperature 35.0 - 110 °C95.0 - 230 °FAverage value: 72.3 °C Grade Count:24
Injection Velocity 200 mm/sec7.87 in/secAverage value: 200 mm/sec Grade Count:4
Drying Temperature 73.9 - 85.0 °C165 - 185 °FAverage value: 79.3 °C Grade Count:15
Moisture Content 0.0300 - 2.00 %0.0300 - 2.00 %Average value: 0.255 % Grade Count:17
Dew Point -17.8 °C0.000 °FAverage value: -17.8 °C Grade Count:3
Injection Pressure 68.9 - 124 MPa10000 - 18000 psiAverage value: 96.5 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 11, Unreinforced
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Nylon 46, Unreinforced

O2600 / 78045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.