MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 301 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D 792
Filler Content 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.17 mm
0.0020 - 0.0040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.3 MPa7000 psiASTM D 638
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %ASTM D 638
Tensile Modulus 3.45 GPa500 ksiASTM D 638
Flexural Strength 75.8 MPa11000 psiASTM D 790
Flexural Modulus 3.10 GPa450 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 - 9.90e+9 ohm-cm1.00e+8 - 9.90e+9 ohm-cmASTM D 257
Surface Resistance 1.00e+9 - 9.90e+10 ohm1.00e+9 - 9.90e+10 ohmESD STM11.11
Surface Resistivity per Square 1.00e+10 - 9.90e+11 ohm1.00e+10 - 9.90e+11 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 246 °C430 - 475 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 110 °C230 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Stat-Rite® M-809 Static Control Acrylic
Trinseo Plexiglas® V825 Acrylic
RTP Company PermaStat® 200 FR Nylon 6/6 (PA) Flame Retardant - Permanently Anti-static - ESD Protection
RTP Company PermaStat® 100 FR Polypropylene (PP), Flame Retardant - Permanently Anti-static - ESD Protection
RTP Company ESD A 100 FR Polypropylene (PP), Flame Retardant - ESD Protection - Static Dissipative

PQZWA1762 / 90904

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.