MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 200 FR Nylon 6/6 (PA) Flame Retardant - Permanently Anti-static - ESD Protection
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D 792
Linear Mold Shrinkage 0.010 - 0.018 cm/cm
@Thickness 3.20 mm
0.010 - 0.018 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.4 MPa6000 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 2.07 GPa300 ksiASTM D 638
Flexural Strength 63.4 MPa9200 psiASTM D 790
Flexural Modulus 1.93 GPa280 ksiASTM D 790
Izod Impact, Notched 0.374 J/cm
@Thickness 3.20 mm
0.700 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 - 9.90e+10 ohm-cm1.00e+9 - 9.90e+10 ohm-cmASTM D 257
Surface Resistance 1.00e+9 - 9.90e+10 ohm1.00e+9 - 9.90e+10 ohmESD STM11.11
Surface Resistivity per Square 1.00e+10 - 9.90e+11 ohm1.00e+10 - 9.90e+11 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 241 - 271 °C465 - 520 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company PermaStat® 301 FR Polycarbonate (PC), ESD Protection - Permanently Anti-static - Glass Fiber - Flame Retardant
RTP Company PermaStat® 100 FR Polypropylene (PP), Flame Retardant - Permanently Anti-static - ESD Protection
RTP Company ESD A 100 FR Polypropylene (PP), Flame Retardant - ESD Protection - Static Dissipative

PQZVA5739 / 120451

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.