MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® MC8100 PC/ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: High Impact, High HDT PC/ABS Sheet (High Gloss)

ALLEN® MC8100 is a general purpose PC/ABS with high impact strength and high heat deflection.

ALLEN® MC8100 meets Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302)

Suggested Applications:

  • Vehicle Interior Trim
  • Covers and Housings
  • Vehicle Exteriors (painted)
  • Instrument Panels

Features:

  • Custom color matching
  • Good forming properties
  • Edge trim easily used for future orders
  • High heat deflection temperature
  • High gloss finish
  • Meets many automotive specifications

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 52.4 MPa7600 psiASTM D638
Flexural Modulus 2.0684 GPa300.00 ksiASTM D790
Izod Impact, Notched  4.27 J/cm
@Temperature -17.8 °C
8.00 ft-lb/in
@Temperature 0.000 °F
ASTM D256
 5.34 J/cm
@Temperature 22.8 °C
10.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 123.9 °C255.0 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104.5 °C220.1 °FUnannealed; ASTM D648
Vicat Softening Point 138 °C280 °FISO 306
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Underwriters Laboratories., Inc®; Component Recognition; UL Standard 94
 
Optical PropertiesMetricEnglishComments
Gloss 80 %80 %60° Angle; ASTM D523
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 204 °C320 - 400 °FForming Temperature
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
 
Descriptive Properties
Motor Vehicle Safety StandardPassesFMVSS 302

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® PC/ABS FR 2810
SEKISUI SPI ALLEN® 2000 PC/ABS
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
LG Chemical LUPOY GP5008A PC/ABS
E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy

PSEKIS024 / 185849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.