MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability. PC/PBT is usually used for automotive applications with good resistance against oils and solvents as well as high impact. PC/PET has an excellent surface and its high heat resistance allows it to be employed in housing for electrical appliances.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.67 MPa9960 psiASTM D638
Elongation at Break 90 %90 %ASTM D638
Flexural Strength 88.29 MPa12810 psiASTM D790
Flexural Modulus 2.403 GPa348.6 ksiASTM D790
Izod Impact, Notched 1.96 J/cm3.67 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® XT XT-100-CX01 PC+PBT
Edinburg Plastics CBT605 PC/PBT
A. Schulman Diamond DIAMALOY 527 PC/PBT Alloy
Avient Edgetek® XT XT-100-BU00 PC+PBT
Avient Edgetek® XT XT-100-BW01 Natural PC+PBT

PEPOLZ039 / 103536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.