MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addovate® SV PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Emulsifier and crosslinker for the production of cellular Vulkollan.

Product information: Addovate SV is used as a crosslinking agent in the manufacture of cellular elastomers based on polyester polyols/Desmodur® 15 by hot casting. The water component serves to promote the propellant effects. To improve dispensing characteristics, a crosslinker should be manufactured containing approx. 10 parts by weight of the polyester polyol also used for the prepolymer (OH value approx. 55). The proportions used should be 2.0 parts by weight Addovate SV to 100 parts by weight polyester polyol - if not otherwise recommended. The crosslinker should also contain the catalyst, e.g. Addocat 105 E (0.01-0.06 parts by weight) or Addocat PP (approx. 0.2 parts by weight to 100 parts by weight polyester polyol). Using a catalyst reduces dwell times in the mold. Cream time can be delayed by adding Addovate DD 1092 (approx. 0.2 parts by weight to 100 parts by weight polyester polyol). The water content of Addovate SV must be taken into account in the recipe.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Viscosity 150 - 250 cP150 - 250 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value 16 - 2016 - 20[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Melting Point -7.00 °C19.4 °FFreezing Point
Boiling Point 100 °C212 °FInitial
Flash Point >= 100 °C>= 212 °FASTM D93, DIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 10.0 - 20.0 °C
6.00 Month
@Temperature 50.0 - 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 49 - 51 %49 - 51 %
 
Descriptive Properties
Appearanceyellowish brown liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU
C.O.I.M. LARIPUR® LPR2202-95A Seal Grade TPU
C.O.I.M. LARIPUR® LPR107-93A Seal Grade TPU
Lanxess Urepan® 50 EL 06 G Polyurethane Rubber
Envalior Akulon® K224-HG6U PA6-GF33, Dry, 33% Glass Filled, Heat Stabilized

PLANY8230 / 208623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.