MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPH 6080 Polypropylene Homopolymer, Cast Film
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.

Polypropylene PPH 6080 can be used as single layer films as well as the core layer of coextruded films, for food packaging, hosiery packaging, shirt packaging, lamination films, ... as well as for stationary supplies.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccISO 1183
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Thickness 50.0 microns1.97 mil
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ISO 2039-2
Film Tensile Strength at Yield, MD 23.0 MPa3340 psiISO 527-3
Film Tensile Strength at Yield, TD 23.0 MPa3340 psiISO 527-3
Tensile Strength, Yield 30.0 MPa4350 psiISO 527-2
Film Elongation at Break, MD 650 %650 %ISO 527-3
Film Elongation at Break, TD 600 %600 %ISO 527-3
Elongation at Yield 10 %10 %ISO 527-2
Tensile Modulus 1.45 GPa210 ksiISO 527-2
Flexural Modulus 1.35 GPa196 ksiISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179
Elmendorf Tear Strength, MD 1.70 g/micron43.2 g/milISO 6383-2
Elmendorf Tear Strength, TD 2.00 g/micron50.8 g/milISO 6383-2
Dart Drop Test 270 g0.595 lbISO 7765-1
Film Tensile Strength at Break, MD 51.0 MPa7400 psiISO 527-3
Film Tensile Strength at Break, TD 42.0 MPa6090 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °F120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F120°C per hour; ISO 752
Vicat Softening Point  87.0 °C
@Load 5.10 kg
189 °F
@Load 11.2 lb
50°C per hour; ISO 306
 152 °C
@Load 1.02 kg
306 °F
@Load 2.25 lb
50°C per hour; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 0.10 %0.10 %ISO 14782
Gloss 91 %91 %at 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 4030 Polypropylene Homopolymer
Total PPH 4026 Polypropylene Homopolymer, Film
Braskem INSPIRE™ 222 Performance Polypropylene Polymer
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy

PTOTAL797 / 130522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.