MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.

EASTALLOY DA003-8999K Polymer is a clear copolyester/polycarbonate alloy. It has excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhanced physical properties advantages.

Applications: Medical

All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness.

Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.

Information provided by Eastman Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ASTM D792 and ISO 1183D
Water Absorption 0.13 %0.13 %24 hour immersion; ISO 62
Moisture Vapor Transmission 6.00 cc-mm/m²-24hr-atm15.2 cc-mil/100 in²-24hr-atmF 372 Test conducted at 38°C (100°F) and 100% relative humidity.
Oxygen Transmission 10.0 cc-mm/m²-24hr-atm25.4 cc-mil/100 in²-24hr-atmASTM D3985
Viscosity Measurement 0.700.700.7 for films per EMN-A-AC-G-V-1
 0.700.70inherent viscosity of pellets
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ISO 2039-2
Tensile Strength, Ultimate 28.0 MPa4060 psiISO 527
Film Tensile Strength at Yield, MD 52.0 MPa7540 psiASTM D882
Film Tensile Strength at Yield, TD 52.0 MPa7540 psiASTM D882
Tensile Strength, Yield 50.0 MPa7250 psiISO 527
Film Elongation at Break, MD 400 %400 %ASTM D882
Film Elongation at Break, TD 400 %400 %ASTM D882
Film Elongation at Yield, MD 4.0 %4.0 %ASTM D882
Film Elongation at Yield, TD 4.0 %4.0 %ASTM D882
Elongation at Break 100 %100 %ISO 527
Tensile Modulus 2.10 GPa305 ksiISO 527
Flexural Yield Strength 68.0 MPa9860 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Secant Modulus, MD 1.90 GPa276 ksiASTM D882
Secant Modulus, TD 1.90 GPa276 ksiASTM D882
Izod Impact, Notched 1.01 J/cm1.89 ft-lb/inASTM D256
 0.370 J/cm
@Temperature -40.0 °C
0.693 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Elmendorf Tear Strength, MD 13.7 g/micron348 g/milASTM D1922
Elmendorf Tear Strength, TD 16.7 g/micron424 g/milASTM D1922
Dart Drop Test 400 g0.882 lbModified 12.7 mm (0.5 in.) dia. head, 127 mm (5 in.) dia. clamp, 660 mm (26 in.) drop. Value at -18°C (0°F) is 500 g.; ASTM D1709A
Film Tensile Strength at Break, MD 59.0 MPa8560 psiASTM D882
Film Tensile Strength at Break, TD 55.0 MPa7980 psiASTM D882
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohm1.00e+16 ohmASTM D257
Dielectric Constant  2.4
@Frequency 1e+6 Hz
2.4
@Frequency 1e+6 Hz
ASTM D 150
 2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm406 kV/inShort Time, 500 V/sec rate-of-rise; ASTM D 149
Dissipation Factor  0.0050
@Frequency 1000 Hz
0.0050
@Frequency 1000 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 143 sec143 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 51.0 µm/m-°C
@Temperature -30.0 - 40.0 °C
28.3 µin/in-°F
@Temperature -22.0 - 104 °F
ASTM D696
Specific Heat Capacity  1.30 J/g-°C
@Temperature 60.0 °C
0.311 BTU/lb-°F
@Temperature 140 °F
 1.76 J/g-°C
@Temperature 100 °C
0.421 BTU/lb-°F
@Temperature 212 °F
 1.88 J/g-°C
@Temperature 150 °C
0.449 BTU/lb-°F
@Temperature 302 °F
 1.97 J/g-°C
@Temperature 200 °C
0.471 BTU/lb-°F
@Temperature 392 °F
 2.05 J/g-°C
@Temperature 250 °C
0.490 BTU/lb-°F
@Temperature 482 °F
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FASTM D648
Vicat Softening Point 85.0 °C185 °FASTM D1525
Glass Transition Temp, Tg 80.0 °C176 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 0.80 %0.80 %ASTM D1003
Gloss 108 %108 %at 45°; ASTM D 2457
Transmission, Visible 85 %85 %per ASTM D1746
 89 %89 %Regular transmittance per ASTM D 1003 Modified.
 91 %91 %Total Transmittance; ASTM D 1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Film Grade
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Overview of materials for Low Density Polyethylene (LDPE), Film Grade

PEA010 / 35220

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.